D 802 | EDCoCr-A-03 | HRc38-47. Resistance to heat, wear and corrosion. Hardfacing of high temperature part such as the edge of thermo-cutter. | ECoCr-A |
D 812 | EDCoCr-B-03 | HRc45-50. Resistance to heat, wear and corrosion. Hardfacing of high temperature part such as internal-combustion engine valve. | ECoCr-B |
D 822 | HRc≥53. Resistance to Wear and heat, bad shock resistance. Hardfacing of rotating blade wheel of boiler. | ||
D 832 | EDCoCr-C-03 | HRc≥50. Wear and heat resistance. Hardfacing of high temperature part such as hot-rolling guided way. | ECoCr-C |
D 842 | EDCoCr-D-03 | HRc28-38. Corrosion and thermo-fatigue resistance, work harding. Hardfacing of hot forging die. |